After a water leaching process, 85.61 of the vanadium from the roasting slag was leached, confirming the sodium oxidation of most of the vanadium oxides to water-soluble sodium vanadate during the roasting process. The total recoveries of iron, vanadium, and titanium were 93.67, 72.68, and 99.72, respectively If you are interested in our products, consult now to get a more favorable price;